Toggle navigation
PiezoMat.org
Browse
Submit Material
login / register
Advertisements
EBL #9
Basic Info
Electric Properties
Elastic Properties
Availabilities & Applications
Basic Information
Density:
ρ :
7.60
g/cm
3
Curie temperature:
T
C
:
320
°C
Material class:
Lead Zirconate Titanate
Reviewed:
Yes
Electric Properties
Piezoelectric charge constant(s)
d
31
:
-135.0
*10
-12
C/N
d
33
:
315.0
*10
-12
C/N
Piezoelectric voltage constant(s)
g
31
:
-10.5
*10
-3
Vm/N
g
33
:
24.6
*10
-3
Vm/N
Dielectric loss factor
tan δ:
0.004
@1000
Hz
Dielectric constant(s)
ε
33
T
:
1450
Coupling factor(s):
k
p
:
0.60
k
31
:
0.34
k
33
:
0.71
Elastic Properties
Mechanical Q factor:
Q
m
:
600
Frequency constant(s):
N
P
:
2110
Hzm
N
T
:
1990
Hzm
Availability
EBL Products, Inc.
www.eblproducts.com
eblpzt.paul@sbcglobal.net