Density:
ρ :
7.80
g/cm
3
Curie temperature:
T
C
:
250
°C
Material class:
Lead Zirconate Titanate
Reviewed:
Yes
Electric Properties
Piezoelectric charge constant(s)
d
31
:
-320.0
*10
-12
C/N
d
33
:
650.0
*10
-12
C/N
Piezoelectric voltage constant(s)
g
31
:
-9.0
*10
-3
Vm/N
g
33
:
19.0
*10
-3
Vm/N
Dielectric loss factor
tan δ:
0.024
@1000
Hz
Dielectric constant(s)
ε
33
T
:
3800
Coupling factor(s):
k
p
:
0.75
k
15
:
0.68
k
31
:
0.44
k
33
:
0.75
Elastic Properties
Mechanical Q factor:
Q
m
:
30
Frequency constant(s):
N
T
:
2030
Hzm
Availability
EBL Products, Inc.
www.eblproducts.com